JPS62287010A - 真空脱ガス炉の補修方法 - Google Patents
真空脱ガス炉の補修方法Info
- Publication number
- JPS62287010A JPS62287010A JP12925786A JP12925786A JPS62287010A JP S62287010 A JPS62287010 A JP S62287010A JP 12925786 A JP12925786 A JP 12925786A JP 12925786 A JP12925786 A JP 12925786A JP S62287010 A JPS62287010 A JP S62287010A
- Authority
- JP
- Japan
- Prior art keywords
- tank
- spraying
- vacuum degassing
- degassing furnace
- repair
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Manufacture And Refinement Of Metals (AREA)
- Treatment Of Steel In Its Molten State (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP12925786A JPS62287010A (ja) | 1986-06-05 | 1986-06-05 | 真空脱ガス炉の補修方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP12925786A JPS62287010A (ja) | 1986-06-05 | 1986-06-05 | 真空脱ガス炉の補修方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS62287010A true JPS62287010A (ja) | 1987-12-12 |
JPH0580526B2 JPH0580526B2 (en]) | 1993-11-09 |
Family
ID=15005090
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP12925786A Granted JPS62287010A (ja) | 1986-06-05 | 1986-06-05 | 真空脱ガス炉の補修方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS62287010A (en]) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN109837362A (zh) * | 2019-04-01 | 2019-06-04 | 山东钢铁集团日照有限公司 | 一种有效减缓rh真空槽槽体变形的方法 |
CN110106315A (zh) * | 2019-04-01 | 2019-08-09 | 山东钢铁集团日照有限公司 | 一种rh真空槽长寿命的控制的方法 |
-
1986
- 1986-06-05 JP JP12925786A patent/JPS62287010A/ja active Granted
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN109837362A (zh) * | 2019-04-01 | 2019-06-04 | 山东钢铁集团日照有限公司 | 一种有效减缓rh真空槽槽体变形的方法 |
CN110106315A (zh) * | 2019-04-01 | 2019-08-09 | 山东钢铁集团日照有限公司 | 一种rh真空槽长寿命的控制的方法 |
Also Published As
Publication number | Publication date |
---|---|
JPH0580526B2 (en]) | 1993-11-09 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Goto et al. | Progress and perspective of refractory technology | |
CN106702077B (zh) | 一种保障转炉高寿命的护炉方法 | |
JPS62287010A (ja) | 真空脱ガス炉の補修方法 | |
US2683032A (en) | Basic lined cupola | |
JPH11229021A (ja) | 転炉型窯炉の内張り耐火物保護方法 | |
KR100332159B1 (ko) | 산화물-기재 내화체의 보수방법 및 이를 위한 분말혼합물 | |
US4468780A (en) | Method of lining a steel-making furnace | |
JPS6156223A (ja) | 転炉のスラグコ−テイング方法 | |
CN214601908U (zh) | 一种混铁车内衬 | |
JP2000313912A (ja) | 転炉スラグコ−ティング方法 | |
JPH0382705A (ja) | 転炉の熱間補修方法 | |
CN115537492B (zh) | 一种转炉底吹护砖和转炉溅渣护炉方法 | |
JP3874216B2 (ja) | 火炎溶射材 | |
JPS5848510B2 (ja) | 耐火材構築物の熱間補修材 | |
JPS6159364B2 (en]) | ||
JPS6054981A (ja) | 高炉出銑樋の火炎溶射吹付補修材 | |
JPS63107873A (ja) | 火炎溶射材 | |
JPS6333077B2 (en]) | ||
JPH09157725A (ja) | 鉄系スクラップの溶解方法 | |
JPS6035037Y2 (ja) | 高温冶金炉における築炉構造 | |
JP3982647B2 (ja) | 火炎溶射材 | |
JPH03134487A (ja) | 不定形耐火物の施工方法 | |
JPS6053273B2 (ja) | 窯炉の火炎溶射補修方法 | |
JPS59220275A (ja) | 溶融金属容器等内壁の補修方法 | |
JPS61213314A (ja) | 精錬用容器のガス吹込み羽口補修方法 |